0% found this document useful (0 votes)
772 views3 pages

Minfm32202 Din 17445 Grade G X5crni13 4 Quenched and Tempered qt1

The document summarizes the properties of DIN 17445 Grade G-X5CrNi13-4 quenched and tempered steel. It is a corrosion and temperature resistant steel used for parts in water power engineering like water turbine casings and guidances, as well as for shipbuilding and compressor construction. The steel has a density of 7.7 g/cm3, hardness of 240-300 Brinell, tensile strength of 760-960 MPa, and contains 12-13.5% chromium and 3.5-5% nickel.

Uploaded by

BS
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
0% found this document useful (0 votes)
772 views3 pages

Minfm32202 Din 17445 Grade G X5crni13 4 Quenched and Tempered qt1

The document summarizes the properties of DIN 17445 Grade G-X5CrNi13-4 quenched and tempered steel. It is a corrosion and temperature resistant steel used for parts in water power engineering like water turbine casings and guidances, as well as for shipbuilding and compressor construction. The steel has a density of 7.7 g/cm3, hardness of 240-300 Brinell, tensile strength of 760-960 MPa, and contains 12-13.5% chromium and 3.5-5% nickel.

Uploaded by

BS
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
You are on page 1/ 3

Metal Steel

DIN 17445 Grade G-X5CrNi13-4 quenched and tempered (+QT1)

Description
G-X 5 CrNi 13 4, for parts in the water power engineering, like water turbine casings and -guidances,
for shipbuilding and building of compressores, cold-tough

Related Standards

EN 10213-4 DIN 17445 EN 10283 EN 10213-1

Properties
General

Density ρ 7.7 g/cm³ at 20 °C

Mechanical

Elongation A 0 - 15 % at 20 °C

Hardness, Brinell HB 240 - 300 [-] at 20 °C

Tensile strength Rm 760 - 960 MPa at 20 °C

Yield strength Rp0.2 Rp0.2 0 - 550 MPa at 20 °C

Thermal

Coefficient of thermal 10.5 1/K at 100 °C


expansion α

Specific heat capacity cp 0.46 J/(kg·K) at 20 °C

Thermal conductivity λ 25 W/(m·K) at 20 °C


Chemical properties

Element Weight % Comment

Cr 12 - 13.5 %

Ni 3.5 - 5 %

C 0 - 0.07 %

Mn 0 - 1.5 %

Mo 0 - 0.7 %

P 0 - 0.04 %

Si 0-1%

S 0 - 0.03 %

This material data has been provided by WIAM.


All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be
stricter whereas others may be outside the bounds of the original standard.
Suggested reading

ASTM A1018

ASTM A108 Carbon and Alloy Steel Bars

ASTM A479 Stainless Steel

ASTM A53 Carbon Steel Pipes

ASTM A564 Stainless Steel Age Hardened

Carbon Steel: Properties, Production, Examples and Applications

Cold Rolled Steels

Electrical Steel: Properties, Types, Production, and Applications

Hot Rolled Steels

Introduction to Steel Grades

Materials Used in Bridges

What is ASTM A36?

What is ASTM A53?

Young's Modulus: Definition, Measurement, and Typical Values

You might also like