37Cr4 ( 1.7034 )
Grade : 37Cr4
Number: 1.7034
EN 10083 - 3 : 2006 Steels for quenching and tempering. Technical delivery conditions for alloy steels
EN 10263 - 4 : 2001 Steel rod, bars and wire for cold heading and cold extrusion. Technical delivery
Standard:
conditions for steels for quenching and tempering
EN 10250 - 3 : 2000 Open steel die forgings for general engineering purposes. Alloy special steels
0.34 - 0.41 max 0.4 0.6 - 0.9 max 0.025 max 0.035 0.9 - 1.2
M e c ha nic a l pr ope r t ie s of gr a de 3 7 Cr 4 ( 1 .7 0 3 4 )
+20°
KV - Impact energy (J) (+QT)
35
Equiva le nt gr a de s of gr a de 3 7 Cr 4 ( 1 .7 0 3 4 )
Warning! Only for reference
USA Germany Japan France England Italy Spain China Sweden Poland Czechia Austria Russia Inter
- DIN,WNr JIS AFNOR BS UNI UNE GB SS PN CSN ONORM GOST ISO
Gr.5135 37Cr4 SCr435H 37Cr4 530A36 38Cr4 38Cr4 35Cr 2245 40H 14140 41Cr4SP 38KHA 37Cr4
38C4 530M36 F1201 40KH
M e c ha nic a l pr ope r t ie s
M e c ha nis c he Eige ns c ha f t e n
Ca r a c t e r is t ique s m e c a nique s
R eH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d�elasticite minimale
R m Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc
He a t t r e a t m e nt c ondit ions
+A Soft annealed
+AC Annealed to achieve spheroidization of the carbides
+AR As rolled
+AT Solution annealed
+C Cold drawn / hard
+CR Cold rolled
+FP Treated to ferrite-pearlite structure and hardness range
+I Isothermal annealing
+LC Cold drawn / soft
+M Thermo mechanical rolling
+N Normalized
+NT Normalized and tempered
+P Precipitation hardened
+PE Peeled
+QA Air quenched and tempered
+QL Liquid quenched and tempered
+QT Quenched and tempered
+S Treated to improve shearability
+SH As rolled and turned
+SR Cold drawn and stress relieved
+T Tempered
+TH Treated to hardness range
+WW Warm worked
+U Untreated
Chemical composition of 37Cr4 (1.7034). Equivalent grades of 37Cr4 (1.7034). Standards of 37Cr4 (1.7034).
Properties of 37Cr4 (1.7034). Hardness of 37Cr4 (1.7034). Strength of 37Cr4 (1.7034). Elongation of 37Cr4 (1.7034).
http://www.steelnumber.com/en/steel_composition_eu.php?name_id=329 2/3
3/20/2014 37Cr4 / 1.7034 - steel equivalent, mechanical properties, chemical composition
© 2011- 2014 All rights reserved. The contents from this site may not be reproduced.
The entire risk as to use of these content is assumed by you the user
http://www.steelnumber.com/en/steel_composition_eu.php?name_id=329 3/3