0% found this document useful (0 votes)
54 views1 page

Getig 80s Ni3 23

This document provides information on Getig 80SNi3 tungsten inert gas (TIG) filler wire. It contains approximately 3.5% nickel and is recommended for both root runs and filling joints. It produces welds with high impact values below -80°C. The wire yields x-ray quality welds and is suitable for welding 3.5% nickel steels where good toughness is required at low temperatures. Its chemical composition and mechanical properties are listed.
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
0% found this document useful (0 votes)
54 views1 page

Getig 80s Ni3 23

This document provides information on Getig 80SNi3 tungsten inert gas (TIG) filler wire. It contains approximately 3.5% nickel and is recommended for both root runs and filling joints. It produces welds with high impact values below -80°C. The wire yields x-ray quality welds and is suitable for welding 3.5% nickel steels where good toughness is required at low temperatures. Its chemical composition and mechanical properties are listed.
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
You are on page 1/ 1

GETIG 80S-Ni3

IDENTIFICATION
Getig 80SNi3, ER 80SNi3

CLASSIFICATION
AWS/SFA 5.28: ER80S-Ni 3

DESCRIPTION
TIG filler wire containing about 3.5 percent Nickel is recommended for root run as well as for joint
filling. The weld metal gives high impact values at subzero temperature up to minus 80°C. Deposited
weld metal is of x-ray quality.

CHEMICAL ANALYSIS (RANGE) %

C Mn Si Cu S P Ni
0.06 - 0.12 0.8 - 1.25 0.40 - 0.80 0.35 max 0.025 max 0.025 max 3.0 - 3.75

MECHANICAL PROPERTIES (RANGE)

UTS (MPa) YS (MPa) EL (%) (L=4D) CVN Impact Value


Temp Joules
550 - 650 470 - 580 24 - 30 -80°C 30 - 90

TYPICAL APPLICATIONS

C-Mn steels where good toughness is required at minus 80°C.

● For welding 3.5 percent nickel steel.


● A 350 Grade LF2, LF5, APL 5LX Grade 65
● General and off-shore engineering, structural and weathering steels, pipe work and pressure
vessels.

SHIELDING GAS : Pure Argon

PACKING PARAMETERS

Size (mm) Length (mm) Packing / Pkt (kg) Packing / Box (kg)
1.6 1000 5 5 x 4 = 20
2 1000 5 5 x 4 = 20
2.40 / 2.50 1000 5 5 x 4 = 20
3.15 / 3.20 1000 5 5 x 4 = 20