100% found this document useful (3 votes)
266 views

Ut.2-Exercise Questionanswer-Asme - Aws

The document discusses ultrasonic testing level 2 training, covering topics like ASME Section V requirements for ultrasonic testing of welds, ultrasonic probe frequencies, calibration procedures, acceptance criteria in codes like ASME and AWS, and evaluating test results.

Uploaded by

Gilang Adi
Copyright
© © All Rights Reserved
Available Formats
Download as PDF, TXT or read online on Scribd
100% found this document useful (3 votes)
266 views

Ut.2-Exercise Questionanswer-Asme - Aws

The document discusses ultrasonic testing level 2 training, covering topics like ASME Section V requirements for ultrasonic testing of welds, ultrasonic probe frequencies, calibration procedures, acceptance criteria in codes like ASME and AWS, and evaluating test results.

Uploaded by

Gilang Adi
Copyright
© © All Rights Reserved
Available Formats
Download as PDF, TXT or read online on Scribd
You are on page 1/ 5

UTRASONIC TESTING LEVEL-II

NDT Q&C Training.


SPECIFIC EXAMINATION-ASME-AWS

Article 4 ASME Sec. V discusses settings on


a. Weld testing uses the Ultrasonic method
b. Ultrasonic testing of welds and dimensioning Indications.
c. Comparing UT admission criteria if necessary, by referencing Code Section.
d. All of the above.

Frequency probes that comply with the provisions of article 4 are


a. 1000000Hz to 5000000Hz
b. 1 MHz to 5 MHz and or adjusted to the grain structure material.
c. Less than 1MHZ or more than 5 MHz
d. Every 2 dB stepping.

Ultrasonic Examination in Article 4 must be carried out in accordance with


a. Purchase Orders
b. Contractor's instruction manual
c. Written procedures that contain at least the following Table T-421.
d. Written procedure approved by engineering.

The instruments permitted according to Article 4 are Ultrasonic instruments


a. Pulse-echo type which is capable of operating at least at 1000KHz up to 5Mhz
b. Pulse-echo type with a capability of less than 5 Mhz
c. Immersion type with operating capability from 1Mhz to 5 Mhz
d. None of the above

ASME Section V is:


a. References Requirements for Ultrasonics
b. Examination Procedures for Ultrasonic Tests of Welds.
c. References Requirements for Ultrasonic Tests.
d. Examination Procedure for Nondestructive Tests

To guarantee ultrasonic coupling on curved test surfaces


a. Then apply a diluted couplant
b. Probe shoes made of plastic were made
c. Tests on test surfaces with a diameter of less than 350mm must be carried out using a probe shoe
with the same contour
d. A probe shoe with a diameter of 350 mm was made

If the test object is made of titanium, the couplant used must not contain halides
a. of 520 ppm
b. less than 520 ppm
c. more than 250 ppm
d. less than 250 ppm

EXERCISE-QUESTION ANSWER
AT23
UTRASONIC TESTING LEVEL-II
NDT Q&C Training.
SPECIFIC EXAMINATION-ASME-AWS

Testing on a test surface with a curved contour of 300 mm, the calibration block used is
a. Diameter 7 in
b. Calibration block 200 in diameter
c. Diameter 180 in
d. You can use a calibration block that is not contoured or just flat.

Ultrasonic Scanning path on the test surface must have an overlap of 10%
Question Type
a. Search unit used during calibration
b. Transducer used for calibration and testing.
c. Probe with a diameter of 10% of the test object
d. All answers are correct.

The permitted movement rate or scanning speed


a. 100mm/min
b. 1500mm/sec
c. more than 150mm/sec
d. None of the above

In ASME Article 4, reflector is the term for artificial defects. Reflectors for UT calibration standards
can be:
a. Defects discovered during inspection
b. Side Drill Hole or Flat Bottom Hole
c. Saw cuts
d. Manually created notches

Scanning sensitivity level in the Distance Amplitude technique must be set:


A. Addition of 3 x 2 dB from the standard block signal
B. Minimum 6 dB of the signal on the reference block
C. No need to add
D. A and B

On the weld test surface that interferes with the UT test then:
a. Adequate surface preparation adjustments for UT must be made.
b. UT testing cannot be performed
c. Re-welding must be done
d. Testing must be carried out with other NDT methods.

In general, both standard blocks and calibration settings must always be the same as the test,
except:
a. Calibration block material
b. Calibration block dimensions
c. Probe used.
d. There is no right answer

EXERCISE-QUESTION ANSWER
AT23
UTRASONIC TESTING LEVEL-II
NDT Q&C Training.
SPECIFIC EXAMINATION-ASME-AWS

Miniature search units are usually used to complete the evaluation of fillet weld inspection results:
a. Less than ¾ in
b. Measuring ¾ in
c. More than 20 mm
d. Less than 2 x 20 mm

AWS D.1.1 is an international code from American Welding Structure which discusses:
a. Requirements for welded steel structures
b. Requirements for Fabrication and Erection of welded metal structures
c. Requirements for NDT Inspection of steel
d. Requirements for NDT Inspection of Structures

AWS D.1.1 – C-6.1 is:


a. Scope for Fabrication
b. Scope for Erection
c. Scope for Inspection
d. Scope is not stated

In C-6.1.1 the Acceptance Criteria are regulated as follows:


a. Acceptance Criteria for static load structures
b. Acceptance Criteria for Repeated Load Structures
c. Acceptance Criteria for Tubular Structures
d. All of the above

In C-6.1.1 regarding acceptance criteria for these structures are fundamentally different in terms of
load:
a. Cyclically
b. Static and Fatigue loading
c. Dynamic
d. There is no right answer

Special UT Technical Provisions are made in writing, as Technical provisions that can be used in the
implementation of UT by different inspectors to achieve:
a. Witten documented
b. To ensure reproducibility of test results
c. Can be reviewed by anyone
d. Results that match the inspector's skills

UT Frequency for using the miniature UT Probe in AWS D.1.1a. Cannot be less than 22.5 Mhz
a. Cannot be less than 22.5 Mhz
b. Must be higher than 2.25 KHz
c. Cannot be more than 2.25 MHz
d. Must be more than 2.25 MHz

EXERCISE-QUESTION ANSWER
AT23
UTRASONIC TESTING LEVEL-II
NDT Q&C Training.
SPECIFIC EXAMINATION-ASME-AWS

Adequate distance calibration must be carried out not only on one standard block thickness, but at
least:
a. Over 2 different standard block thicknesses
b. Over 3 different standard block thicknesses
c. Over 4 different standard block thicknesses
d. All of the above

The provisions for carrying out laminar checks on base metal are not to check the acceptability of
the base metal, but rather:
a. Determines the base metal's ability to accept a particular UT test
b. Determine the dimensions of material defects
c. Create a test reference
d. Look for defects that are half a lamda in size

In IIW reference block calibration, longitudinal mode, settings are made to:
a. Distance Calibration, Horizontal Linearity Qualification
b. Amplitude, Gain Control (attenuation) Qualification
c. Resolution, amplitude
d. All answers are correct

According to Table 6.7 AWS D.1.1, 2015, the transducer angle is the best and most accurate in
evaluating discontinuity.
a. 45ᵒ
b. 60ᵒ
c. 70ᵒ
d. All of the above

The major dimensions of the discontinuity in the table should be oriented:


a. Normal terhadap arah gabungan tegangan sisa atau tegangan yang diberikan
b. Mendekati normal arah gabungan tegangan sisa atau tegangan yang diberikan
c. Arah yang sangat membahayakan terhadap keutuhan pengelasan
d. All of the above.

EXERCISE-QUESTION ANSWER
AT23
UTRASONIC TESTING LEVEL-II
NDT Q&C Training.
SPECIFIC EXAMINATION-ASME-AWS

Many false indications are caused by fit-up problems or the connection of two plates of different
thicknesses. Based on the picture below, a root discontinuity (IS) such as a crack or lack of fusion
appears when tested from point A. To confirm this false indication, do:

a. Test from point A1


b. Test along the length of the weld starting at point A
c. It can be ascertained that IS is a true indication
d. Test at a 45ᵒ angle
From the picture above, in general the distance path from A to IS is the distance where the wave
travels until it finds its first reflector, this distance is called:
a. 1 Skip
b. If the plate thickness is 1 inch then the distance is sin Ɵ x thickness
c. 2 Skip to point A1
d. 1 Leg

Dari gambar-1, diatas, Jika defect L menghasilkan indikasi dari titik A1, maka dapat
dipastikan bahwa IS adalah bukan discontinuity :
a. Not true
b. Loss of L indication from point A1, is evidence that IS is a mere reflector source.
c. Correct
d. No answers are correct.

EXERCISE-QUESTION ANSWER
AT23

You might also like