Stainless FC Tig
Stainless FC Tig
Procedures may vary with change in position, base metals, filler metals, equipment and other
changes.
Chemistry
Grade 1) Intended Use
C Cr Ni Mo
R308L 0.03 18.0-21.0 9.0-11.0 0.50 Welding of 18Cr & 8Ni such as 304, 304L
R308H3 ) 0.04-0.08 19.5-22.0 9.0-11.0 0.50 Welding of 18Cr & 8Ni such as 304, 304H
R309L 0.03 22.0-25.0 12.0-14.0 0.50 Welding of carbon steel to austenitic stainless
R316L 0.03 17.0-20.0 11.0-14.0 2.0-3.0 Primarily use on 316 or 316L
R347 2) 0.08 18.0-21.0 9.0-11.0 0.50 Primarily use on 347
1) All grades has the following : Mn=0.50-2.5, Si=1.2, P=0.04, S=0.03 Cu=0.50 Single values are maximum
2) R347 also has Cb+Ta =8xCmin. -1.0 max.
3) R 308H is not listed in AWS; the chemistry is from E308HTO-3 per AWS A5.22 which provides higher strengths at elevated
temperatures.
AVAILABLE SIZES: TFT 308L= Rods of 3/32, 1/8
TFT 308H= Rods of 3/32, 1/8
TFT 309L= Rods of 3/32, 1/8
TFT 316L= Rods of 5/64,3/32, 1/8
TFT 347 = Rods of 3/32, 1/8
SPECIFICATIONS: Washington Alloy per AWS for stainless flux cored rods chemistry only
Washington Alloy Company believes that all information and data given is correct. Use this information to assist in making your
own evaluations or decisions and this information should not be mistaken as an expressed or implied warranty. U.S. ALLOY CO.
assumes no liability for results or damages incurred from the use of any information contained herein, in whole or in part.
.