ATARFIL HD M GRI, ASTM USA ENG - Geomebrana

Uploaded by

esamaniegr
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as PDF, TXT or read online on Scribd
You are on page 1/ 1

ATARFIL HD

ATARFIL HD geomembranes are manufactured from best in class Polyethylene (HDPE) resins coupled with specific antioxidant
package by the most advanced in-house flat-die technology. This result in a quality and consistency product with maximum durability
and long term performance. Scoring the highest STRESS CRACK RESISTANCE value in the industry, together with an unrivalled
mechanical and chemical properties, makes it the best choice for any application.

PHYSICAL PROPERTIES ENDURANCE PROPERTIES


Property Test Method Unit Value Frequency1 Property Test Method Unit Value Frequency1
Density of Raw
ASTM D 792 g/cc ≥ 0.932 - Stress Crack ASTM D 5397/
Material h ≥ 3,000 200,000 lb
Resistance ISO18488(4)
ASTM D 1238
Melt Flow Index g/10 min ≤ 0.40 1 per batch
(190ºC/2.16 Kg) Oxidative Induction
Time (OIT)
Density of 0.946 ± min 200,000 lb
ASTM D 792 g/cc 200,000 lb Std OIT ASTM D 8117 ≥ 120
Geomembrane 0.004
HP OIT ASTM D 5885 ≥ 500
Carbon Black Oven Aging at 85ºC
ASTM D 4218 % 2.0 – 2.5 Per roll ASTM D 5721 Per
Content HP OIT % retained % ≥ 80
ASTM D 5885 formulation
Carbon Black after 90 days
ASTM D 5596 Category Note 3 45,000 lb
Dispersion
UV Resistance
ASTM D 7238 Per
Dimensional ASTM D 1204 HP OIT % retained % ≥ 75
% ± 1.5 Per day ASTM D 5885 formulation
Stability (100ºC/1h) after 1600h

Low Temperature No Per


ASTM D 746 -
Brittleness (tª -70ºC) cracks formulation

MANUFACTURING PROPERTIES
Property Test Method Unit Value Frequency1
Thickness (Nominal) mil (mm) 30 (0.75) 40 (1.00) 60 (1.50) 80 (2.00) 100 (2.50) 120 (3.00)
Thickness (Minimum Average) ASTM D 5199 mil (mm) 30 (0.75) 40 (1.00) 60 (1.50) 80 (2.00) 100 (2.50) 120 (3.00) Per roll
Thickness (Minimum Individual Value) mil (mm) 27 (0.68) 36 (0.90)54 (1.35) 72 (1.80) 90 (2.25) 108 (2.70)
Mechanical Properties2
Tensile Strength at Yield lb/in (N/mm) 63 (11) 84 (15) 126 (22) 168 (29) 210 (37) 252 (44)
Elongation at Yield ASTM D 6693 % ≥ 13
20,000 lb
Tensile Strength at Break Type IV lb/in (N/mm) 114 (20) 154 (27) 228 (40) 304 (53) 382 (67) 456 (80)
Elongation at Break % ≥ 700
Tear Resistance ASTM D 1004 lb (N) 21 (93) 28 (125) 42 (187) 56 (249) 70 (311) 84 (374) 45,000 lb
Puncture Resistance ASTM D 4833 lb (N) 60 (270) 78 (350) 110 (490) 144 (640) 182 (810) 220 (980) 45,000 lb

STANDARD SIZES
04042022

Thickness [mil (mm)] 30 (0.75) 40 (1.00) 60 (1.50) 80 (2.00) 100 (2.50) 120 (3.00)
Roll Width [ft (m)] Roll Length [ft (m)]
19.7 (6) 1332 (406) 999 (304.5) 663 (202) 498 (152) 399 (121) 333 (102)

(1) Indicated frequency is minimum.


(2) Indicated minimum values with 97.5% confidence level.
(3) Carbon black dispersion (only near spherical agglomerates) for 10 different views: in Categories 1 or 2 only.
(4) Additional information regarding correlation between Test Methods ISO 18488 and ASTM D 5397 available upon request.

This product specifications meet or exceed GRI GM13.


The information contained in this document is provided for informational purposes only. Atarfil reserves the right to change this information without prior notice.

ATARFIL HD M GRI, ASTM USA ENG Rev 2