Understanding Heat Shrinks 03
Understanding Heat Shrinks 03
• Minimum shrink
temperature: 70˚C
• Full recovery
temperature: Above
110˚C
Product Description
ATTRIBUTE 1
It is a high shrink ratio military grade heat shrinkable tubing made of 135˚C polyolefin material. In
addition to the normally reliable insulation protection, the high shrink ratio is more suitable to be
applied to the product with irregular outer diameters and providing more comprehensive coverage.
General Specifications
Technical Data
Specification
Property Test Method Typical Value
Requirement
ASTM D2671
Tensile strength after aging 70% of initial value ≥80%
(158˚C/168 hrs)
ASTM D2671
Elongation at break after aging ≥100% ≥200%
(158˚C/168 hrs)
ASTM D2671
Heat shock No cracking No cracking
(200˚C/4 hrs)
ASTM D2671
Low temperature flexibility No cracking No cracking
(-55˚C/4 hrs)
AC2500V/60S
Dielectric voltage withstand ASTM D2671 No breakdown
No breakdown
Mechanical Specifications
Chemical Properties
Transparent Stability 175°C x 24 hours
Fluid Resistance After immersion at 24°C x 24 hours
Flammability Flame Retarded
Tensile Strength 10.3MPa (min.)
Dielectric Strength 19.7KV/mm
Corrosion Non-corrosive
Water Absorption < 0.5%