Plastering
Plastering
PLASTERING
Applying mortar coats on the surfaces of walls, columns, ceiling etc. to get smooth finish is
termed as plastering. Mortar used for plastering may be lime mortar, cement mortar or lime-
cement mortar. Lime mortar used shall have fat lime to sand ratio of 1: 3 or 1: 4. If hydraulic
lime is used mix proportion (lime: sand) is 1 : 2. Cement mortar of 1: 4 or 1: 6 mix is very
commonly used for plastering, richer mix being used for outer walls. To combine the cost
effectiveness of lime mortar and good quality of cement mortar many use lime-cement mortar
of proportion (cement : lime : sand) of 1 : 1 : 6 or 1 : 1 : 8 or 1 : 2 : 8.
Method of Plastering:
The plastering could be done on the surfaces either in one, two and three coats. The
plasterings for two coats are as follows:
• The mortar joints are racked out to a depth of 20 mm and surface is cleaned and well
watered. If it is found that the surface to be plastered is very rough and uneven, a primary
coat is applied to fill up the hollows before the first coat of plaster is put on the surface.
• The first coat of plaster is now applied on the surface. The usual thickness of first coat for
brick masonry is 9 mm to 10 mm. In order to maintain uniform thickness, the screeds are
formed on the wall surface by fixing dots.
• The cement mortar is placed between successive screeds and surface is properly finished.
The second coat is applied after six hours and thickness of second coat is 3 mm to 2 mm.
The completed work is allowed to rest for 24 hours and then, the surface is kept well
watered for rest of week.
For plastering in three coats are similar to two coats. The thickness of first coat (rendering
coat) 9 to 10 mm, second coat (rendering coat) 9 to 10 mm, and third coat (setting coat)
thickness around 3 mm.
The techniques for plastering various surfaces:
Initially, the Surface where plastering is to be done will be cleaned. Level pegs on walls will
be fixed with reference to the off lines to brick walls set out in floors. (Using centre plumb
bob and nylon thread). All the brick walls will be watered before pasting mortar on walls.
First coat mortar filling (1:4 Cement and Sand) up to 15 mm will be applied on surfaces
where required mortar thickness exceed 25mm. Walls and columns will be plastered 1:4
Cement and Sand to achieve semi rough finished surface. Vertical joint of structural columns
/ walls & brick walls will be treated by fixing 200mm width chicken mesh with wire nails /
concrete nails by centering the mesh to the vertical wall joint. All the embedded service lines
and provisions (Conduits, Boxes and etc. ) will be completed on brick walls and check with
the MEP drawings. Joints between walls and beams will be formed up to a maximum of
20mm and will be sealed using 30 minutes fire rated flexible filler. (Material descriptions will
be submitted for the approval of the Engineer) Internal plastering on surfaces of concrete
columns, beams & walls which are aligned with surfaces of brick walls will be plastered and
other concrete surfaces will be finished with cement base easy plaster. (Material descriptions
will be submitted for the approval of the Engineer).
Alignment and fixing level pegs on external wall surfaces will be done using the surveying
instrument / centre plumb bobs. Projections on the wall surfaces will be chipped off and
cleaned after completing the level pegs on walls. First coat mortar filling (1:4 Cement and
Sand) up to 15 mm will be applied on surfaces where required mortar thickness exceed
25mm.Cement paste on concrete surfaces will be applied to improve the bonding of plaster to
the concrete surfaces. Maximum width of 20mm horizontal grooves between walls and
beams will be formed by cutting using grinders with diamond wheels after plastering the wall
surface. This groove will be filled with approved weather sealant. External wall plaster will
be finished with rough surface. 1:10 slope at the external side of the window sill will be
formed while plastering the window reveals.
• Soffit Plastering / Soffit Finishing with Cement Based Easy Plaster
The slab soffits and beams' sides and soffits which are to be smooth surfaced painted finished
will be smoothen with easy plaster (Material literature will be submitted separately) and
places where concrete surfaces are uneven, will be roughen & leveled with cement and sand
mortar plaster before applying easy plaster to make surface smooth.
• There are numerous plastering techniques used to plaster ceilings and walls. It all depends
on the requirements of the client as well as the nature of the area that needs plastering.
Let’s take a look at some general plastering techniques:
• Over the years, traditional Melbourne homes made use of wet plastering to ensure a
smooth finish to ceilings and walls. During the last 3 to 4 decades, dry plastering or dry
lining plastering techniques are being used instead. This method is favoured due to the
ease of using a plasterboard. After all, plasterboards are solid and available in sheet form
in standard sizes of around 2.4 x 1.2 meters. Plasterers Melbourne found it a breeze to
handle and put plaster on. What is more, dry lining is a complete dry procedure which
allow plasterers to quickly fix any mishaps. Paint can easily be applied to any surface to
ensure a warm and welcoming finish.
• The biggest reason why most builders or plasterers prefer using dry lining is due to the
speed of applying it and the load being reduced on structures of any kind. As plasterboard
walls are lightweight, they offer better flexibility when it comes to planning interior or
exterior spaces on the drawing board. In addition, dry lining is a plastering technique that
saves you money and time. Yet another reason why it is the most preferred plastering
method as far a construction work in timber frames are concerned.
Wet Plastering
• Known to be the most common of all plastering techniques used is wet plastering. It
enables experiences plasterers Melbourne to obtain a clean and smooth finish by covering
any surface in need of plastering with mortar, then smoothening it using trowels. Dried
wet plastered surfaces can be painted or papered according to individual preferences. Like
most plastering techniques, it requires skilled plasterers and enough drying time. Wet
plastering is prone to shrinkage, cracks, and often times in need of re-plastering in order
to cover any cracks.
Defects in Plastering
• The brickwork and plastering should be carried out in the best workmanship manner.
• The bond of brickwork should be maintained properly.
• The efflorescence is removed by rubbing brushes on damaged surfaces. A solution of one
part of HCl or H2SO4, and five parts of clean water is prepared and it is applied with the
help of brushes on affected area. The surface is washed and cleaned with water.
• The bricks of superior nature should only be used for the brick work.
• The water free from salts should be used for brick work and plastering work
• The surface to be plastered should be well watered so that it may not absorb water from
plaster.
• The damp- proof courses should be provided at convenient places in buildings.
• The overall construction should be such that the penetration of moisture is prevented.
• The fresh plastered surface should be protected from surplus quantity of water such as
rain and excessive heat such as sun.