Function Improves wet fastness properties of cellulosic fibers, dyed and printed
with substantive and reactive dyestuffs, as well as of dyed and printed
WO and silk fibers
Lava Fast CNC is very suitable for improving the wet fastness properties
of dyed and printed WO and silk fibers, it is free of formaldehyde and
epihalogen hydrin compounds, the influence on shade and light fastness
is negligible.
Lava Fast CNC shows a good compatibility with non-ionic and cationic
products. Precipitations will, however, occur with anionic products.
An aftertreatment with Lava Fast CNC will not noticeably impair handle
and sewability.
Dyeing/Printing
Exhaust method
Aftertreatment of CEL
pH 5 - 6, 20 - 30 min 40°C.
The above stated for CO dyeing is also applicable for the one-bath two
step method with Lava Fast CNC and a cationic softener.
Padding
DyStar Kimya Sanayi ve Ticaret Ltd. Sti This information and our technical advice - whether verbal, in writing or by
Mecidiye Mah.Cenap Sahabettin Sok.No:24 way of trials - are given in good faith but without warranty, and this also
34718, Kosuyolu / Kadikoy applies where proprietary rights of third parties are involved. Our advice
Istanbul - Turkey does not release you from the obligation to check its validity and to test our
products as to their suitability for the intended processes and uses. The
Telephone +90 216 544 15 00
application, use and processing of our products and the products
Fax(sales) +90 216 339 90 48 manufactured by you on the basis of our technical advice are beyon d our
Fax (marketing) +90 216 339 90 63 control and, therefore, entirely your own responsibility. Our products are
[email protected] sold in accordance with our General Conditions of Sale and Delivery .
www.DyStar.com